Design and Fabrication of 4-layer Hybrid RO4450F/RO4350B RF PCB design requirements, the following analysis covers: 50Ω trace width, mixed-material lamination process, drilling and hole metallization

Brand Name: Rogers Model Number: RO4350B+RO4450F

Product Description

 

One Stackup Parameter Inconsistency Needs Clarification First

The stackup diagram specifies “two 0.102 mm RO4450F prepregs,” but the official RO4450F specification is 4 mil (0.101 mm) per sheet, and under recommended lamination conditions, the nominal pressed thickness per sheet is 0.101 mm. Two sheets stacked together should theoretically press to about 0.202 mm, which is essentially consistent with the 0.204 mm shown in the stackup diagram (the difference comes from copper distribution and resin fill during lamination).

 

However, the total thickness needs to be recalculated:

Design and Fabrication of 4-layer Hybrid RO4450F/RO4350B RF PCB design requirements, the following analysis covers: 50Ω trace width, mixed-material lamination process, drilling and hole metallization

 

The 0.766 mm in the stackup diagram differs from the theoretical value by 0.002 mm, which is within a reasonable engineering rounding range; the finished thickness specification of 0.8 ± 0.1 mm also covers this range. Note that the pressed thickness of each RO4450F sheet varies with inner-layer copper distribution. If the copper area on IN1/IN2 is large, the actual fill thickness will be slightly less than 0.101 mm per sheet. It is recommended to specify to the PCB fabricator that “the nominal pressed thickness of the prepreg should be calculated as 0.202 mm” rather than using 0.204 mm.

 

 

Design and Fabrication of 4-layer Hybrid RO4450F/RO4350B RF PCB design requirements, the following analysis covers: 50Ω trace width, mixed-material lamination process, drilling and hole metallization

 

50Ω Microstrip Width (TOP Layer, Referenced to IN1)

The RF traces on the TOP layer use IN1 as the reference ground plane, with a dielectric of 0.254 mm RO4350B + 0.035 mm copper thickness. For RO4350B with Dk ≈ 3.48 (typical at 10 GHz) and 1 oz finished copper, the 50Ω microstrip width is approximately 0.56 mm. Some measured reports use 0.58 mm for the same stackup, with the difference coming from Dk batch variation and copper thickness definition.

 

Design recommendations:

Use 0.56 mm for the initial routing, but do not treat the datasheet nominal Dk as the final basis. Production batches may have Dk varying between 3.43 and 3.53. A Dk decrease of 0.05 shifts the 50Ω line impedance by about +1.5Ω, corresponding to a line width deviation of about 0.02 mm.

 

On the impedance control drawing sent to the PCB fabricator, clearly state: “TOP-layer RF traces target 50Ω, referenced to IN1; line width shall be based on the fabricator’s recheck using the measured batch Dk; impedance tolerance ±10% (tighten to ±5% for millimeter-wave applications).”

 

Require batch-by-batch TDR verification of finished boards, not just first-article confirmation.

 

 

Mixed-Material Lamination: Key Control Points for RO4350B + RO4450F

RO4350B has a Tg >280°C, much higher than ordinary FR-4. During mixed lamination, the two materials soften differently during heating. As the dedicated bonding prepreg, RO4450F’s resin system reaches its lowest viscosity in the 100–120°C range, which is the key window for flow and fill.

 

Recommended lamination profile principles:

Heating rate ≤ 3°C/min; a more conservative approach is 1.2–2.0°C/min. Heating too fast causes uneven RO4450F resin flow and forms voids between layers.

 

Set a temperature hold plateau in the 140–170°C range so that softening/flow of the RO4350B core and RO4450F prepreg become more synchronized, reducing interlayer stress.

 

Peak temperature 190–200°C, hold for 30–60 min to ensure full cure of RO4450F.

 

Apply pressure in stages: apply initial pressure around 100°C for tacking, then adjust the main pressure stage according to board thickness and copper distribution to avoid insufficient resin fill caused by local pressure deficiency.

 

Inner-layer pretreatment: Before lamination, the IN1/IN2 copper surfaces should undergo oxide treatment (brown oxide/black oxide or an alternative process) to improve mechanical adhesion to RO4450F. Before stacking, inner-layer cores are recommended to be baked at 115–125°C for 15–30 min to remove absorbed moisture.

 

Drilling and Hole Metallization: RO4000’s “Simplified Items” and “Cannot-Be-Omitted Items”

 

What Can Be Simplified

The RO4000 series resin system has high Tg and a low tendency to form smear during drilling, so a dedicated desmear step is usually not required. This is fundamentally different from PTFE materials, which require sodium-naphthalene treatment or plasma activation. If drilling parameters are reasonable, the hole walls can go directly into the copper deposition process.

 

What Cannot Be Omitted

Drill bit life must be set separately: the ceramic filler in RO4350B accelerates drill bit wear, so FR-4 hit counts cannot be carried over. It is recommended to base bit changes on hole-wall quality rather than a fixed hit count. The typical hole-wall roughness of RO4000 is 8–25 μm, and this roughness itself is beneficial for hole-wall adhesion to the plated copper.

 

If smear occurs (usually caused by excessive feed rate or excessive drill bit wear), use alkaline permanganate or CF₄/O₂ plasma. Etch-back is not recommended, because the RO4000 ceramic filler system is sensitive to over-etching.

 

Before copper deposition, a micro-etch treatment (e.g., sulfuric acid/hydrogen peroxide system) is recommended to roughen the smooth RO4350B surface and improve plating adhesion.

 

Surface Finish and Final Inspection

ENIG (electroless nickel/immersion gold) is suitable for RO4350B. In mixed-material RF boards, the nickel layer acts as a diffusion barrier, while the gold layer provides solderability and oxidation resistance. The gold thickness is recommended to be controlled within the conventional range of 1.5–3 μm; excessively thick gold increases the skin-effect contribution to high-frequency loss.

 

Final inspection should include at least:

TDR impedance testing: cover the 50Ω RF traces on the TOP layer and record measured impedance curves;

 

Hole-wall cross-sectioning: confirm continuity of the copper deposition/electroplating layers and check for voids caused by residual smear;

 

Interlayer adhesion: for mixed-material boards, thermal stress testing (e.g., 288°C solder float) is recommended to observe any delamination or blistering.

 

Manufacturing Specification Summary

Item Specification
Layer count 4 layers
Stackup TOP Cu 1 oz / RO4350B 0.254 mm / IN1 Cu 1 oz / RO4450F ×2, pressed thickness approx. 0.202 mm / IN2 Cu 1 oz / RO4350B 0.168 mm / BOT Cu 1 oz
Finished board thickness 0.8 ± 0.1 mm
50Ω target line width ≈ 0.56 mm (subject to fabricator recheck using measured Dk)
Impedance tolerance ±10% (±5% for high-frequency/millimeter-wave applications)
Lamination peak temperature 190–200°C, hold for 30–60 min
Heating rate ≤ 3°C/min; recommended 1.2–2.0°C/min
Desmear Usually not required; if smear is present, use alkaline permanganate or plasma; no etch-back
Surface finish ENIG, gold thickness 1.5–3 μm
Solder mask/legend Green solder mask, white legend; no solder mask or legend on BOT layer
Dimensions 50 mm × 60 mm, 1 piece
Special requirements Batch-by-batch TDR impedance report; provide RO4350B batch Dk certificate

 

If further refinement is needed, the next step can be: back-calculate the actual pressed thickness of RO4450F using the IN1 copper thickness and actual copper area, or provide a skin-depth and loss budget for the TOP-layer RF traces at the specific frequency. Both directly affect the final impedance and insertion-loss metrics.

 